Millman972g
Member
Pretty mucha newbie question about...How much silver do I use to enquart with the gold. Is it a different amount based on the amount of karat scrap. Do I inquart if its gold filled scrap?
Welcome to us.Pretty mucha newbie question about...How much silver do I use to enquart with the gold. Is it a different amount based on the amount of karat scrap. Do I inquart if its gold filled scrap?
You need to know how much pure gold you have in the karat gold. Then add enough to the weight of the karat jewelry so the pure gold will be 25% of the alloy you will make.Pretty mucha newbie question about...How much silver do I use to enquart with the gold. Is it a different amount based on the amount of karat scrap. Do I inquart if its gold filled scrap?
That's all I needed thanks for the help!Welcome to us.
Pleas write your text in proper English, we have members that rely on translators and slang and lingo do not translate well.
Inquarting is to bring the karat of the Gold to 6 (25%) so it is very much about the karat, yes.
Here is for your studies:
We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/
Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/
Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
Enter your email address to join: