This is a cylindrical cell that I built with PVC pipe 6 inches in diameter and 40 inches high overall.
The main body is 28 inches long heads are 12 inches high each.
The cathode is stainless steel plate 304 of 0.15 mm thick and is connected with a bolt 3/4 stainless steel also.
The anode is constructed of 1 m from 304L stainless steel pipe with a welded steel disc at one end and a thread of 1 inch to close the cell in the other.
The anode or central axis is connected to the positive pole of the power supply and the plate cylinder acts as cathode and is connected to the negative pole of the power supply.
Feeding the lower and upper outlet are tangential and have a diameter of 1 1/2 inch.
The working voltage of the cell is 2.2 and the silver deposit has reached 3 kg. for each cell.
The flow of solution in the cell is 60 lt / min.
The main body is 28 inches long heads are 12 inches high each.
The cathode is stainless steel plate 304 of 0.15 mm thick and is connected with a bolt 3/4 stainless steel also.
The anode is constructed of 1 m from 304L stainless steel pipe with a welded steel disc at one end and a thread of 1 inch to close the cell in the other.
The anode or central axis is connected to the positive pole of the power supply and the plate cylinder acts as cathode and is connected to the negative pole of the power supply.
Feeding the lower and upper outlet are tangential and have a diameter of 1 1/2 inch.
The working voltage of the cell is 2.2 and the silver deposit has reached 3 kg. for each cell.
The flow of solution in the cell is 60 lt / min.