ericrm said:
i cant talk for others
but personnaly i will not broke mine in piece anymore,
i will remove the lid end put them on the side
may i ask if you have found any silver or palladium in your nitric acid?

I don't have test solution for silver yet, bet stannous test did show a slight positive for palladium.
 
Hello all , how are tricks?
I hope all is well!
I just wanted to quickly say nice work to the winners , and nice work Chris for putting on another contest! 8)
All the best everybody , and kind regards ,
Chris :mrgreen:
 
Hey Eric,
Your welcome, no worries, let us know what you yield out of it.

Thanks,
Chris
 
At around 4 grams yeild for 4 lbs or 64 that says to me either you are not getting out what you shold be or the list http://www.scribd.com/doc/45189378/Gold-Content-List-in-CPU-Chips is way off as their yeald calculates to 7.68 grams. I suspect that he could have gotten a little more, but that the list sighted is a bit off!

I know this is late, but I hope someone else doesn't get fooled by that list.
 
That list is a little too generous and somewhat inaccurate. I wouldn't suggest to buy scrap according to it, but it does give the general idea of what worth more and what worth less.
 