samuel-a
Well-known member
- Joined
- Oct 7, 2009
- Messages
- 2,190
samuel-a said:Rodthrower18
This is not from n/s bridge, just a common Black IC.
I'll upload one of the n/s bridge later if theres anything to see.
resabed01
The picture was taken after a chemical treatment.
Samsamuel-a said:goldenchild
I believe they are soild gold at high purity, GSP once mentioned they are one of the very few items in electronics which are made of high purity gold.
maynman1751
No, i did not use nitric acid.
With your permission, i would prefer not to disclose how i did it, for the moment.
Few days ego i had a... "2 + 2" moment while in my lab... and i found a relatively "easy" way to strip the chips clean.
I'm now working to develop it into a single flowing process, with the hope of keeping things both cost effective and SAFE.
This method may be somewhat dangerous and controversial, i'm sure not everybody will approve it, so, for the moment, i prefer not to induce anyone to try and possibly hurt himself for an untested and unproven process.
Until than, i'll keep it to myself, with the hope you will understand.
What goldenchild said!!! :mrgreen:goldenchild said:If you could ramp this process up to have the capability of processing 1 pound batches with an end result like in your latest picture... I would gladly pay for that information.