I just finished trimming fingers from 441 RAM sticks and 21 mini RAM sticks for a weight of 572g. I also trimmed larger fingers from 10lbs of blank PCB's for a weight of 242g. I'm so excited to be getting to work on this stuff!
I'm in the middle of reading Hokes book on refining and I'm not going to start any reactions until I'm finished absorbing more information so in the meantime, I'll be stripping all the flat packs and MLCC's from the RAM sticks.
My hands hurt from trimming all of these! 😅
 