So I’ve gone over this in my head multiple times and I feel I must be missing something. So if you go to boardsort or any other ewaste buying website, the price they pay for ceramic CPUs is way higher than the price of gold tabbed BGAs and this baffles me, because it seems that no matter how I calculate it, (using data from many different resources, especially these forums) the tabbed BGAs appear to be far superior to any ceramic CPUs in regards to yields. For example, even with the fiber still attached, I’ve noted people yielding up to 5 grams of gold per 1 kilogram of chips. Counting just the chips and no fiber, up to 10 grams per kilogram of chips. While on the other hand, the highest yield I can find data for with even the best ceramic CPUs is anywhere from 2-4 grams per lb or 4-8 grams per kilo (just rough estimates from things I’ve taken note of)
Now boardsort pays 15$/lb of gold cornered BGAs, and anywhere from 67-190$/lb of ceramic CPUs depending on the type of cpu and that’s not counting the lower grade ones like k6.
What gives? Am I forgetting to calculate something? Just surprised they only pay 15$ per lb of the tabbed BGAs
Now boardsort pays 15$/lb of gold cornered BGAs, and anywhere from 67-190$/lb of ceramic CPUs depending on the type of cpu and that’s not counting the lower grade ones like k6.
What gives? Am I forgetting to calculate something? Just surprised they only pay 15$ per lb of the tabbed BGAs