¿Quién sabe dónde conseguir equipos para recuperar y refinar Rutenio y Osmio?
 
¿Quién sabe dónde conseguir equipos para recuperar y refinar Rutenio y Osmio?
For quantities of ruthenium and osmium that you can have, an ordinary standard-equipped lab will be sufficient. No special equipment is required.
 
For quantities of ruthenium and osmium that you can have, an ordinary standard-equipped lab will be sufficient. No special equipment is required.
One would need some stringent safety protocols though, and proper training of the ones working there.
 
If my memory serves me correctly staff who refine osmium in South Africa are only allowed to do so for a short period of time and only once , perhaps if that’s correct I would rethink your ideas.
 
It’s to avoid the permanent deposit of osmium dioxide in your cornea and progressive loss of vision.

That, coupled with its near worthlessness and illiquidity make it more nuisance than revenue source.

Back, Jon?
 
It’s to avoid the permanent deposit of osmium dioxide in your cornea and progressive loss of vision.

That, coupled with its near worthlessness and illiquidity make it more nuisance than revenue source.

Back, Jon?
Very dangerous, but then how do they do it in the world? Nobody talks about this, they just say that it is very dangerous.
 
It’s to avoid the permanent deposit of osmium dioxide in your cornea and progressive loss of vision.

That, coupled with its near worthlessness and illiquidity make it more nuisance than revenue source.

Back, Jon?
Yeah. It took a few years to develop and build the electronics recycling plant Lou. The mechanical/optical/gravity/size separation took a boatload of R and D.
 
Yeah. It took a few years to develop and build the electronics recycling plant Lou. The mechanical/optical/gravity/size separation took a boatload of R and D.

Good to see you back Jon - often wonder how you are doing (& now we know) ;)

A few know but it's not been publicised however Deano, Nickvc, Goran, Kurtak, and Patnor are all spending a week together here in the UK having a bit of a "get together."

Above quote from this thread -----

https://goldrefiningforum.com/threads/false-iridium-finds.28009/#p295508

That "get together" was one of the highlights of my being a member here - I was honored to be invited & spend a week with some of my mentors

Kurt
 
Yeah. It took a few years to develop and build the electronics recycling plant Lou. The mechanical/optical/gravity/size separation took a boatload of R and D.
I bet.

Please play nice here and I imagine you are most welcome to stay, I'm sure I'm speaking for most when I say it's glad to have you back with all the dear bought experience.
 
Spaceships is back in orbit!

What happened to all of the old spaceships posts?
I think they are renamed with Anonymous as all other posts that have had their users purged.

edited to correct spelling of anonymous
 
Last edited by a moderator:
Spaceships is back in orbit!

What happened to all of the old spaceships posts?

I think they are renamed with Antonymous as all other posts that have had their users purged.
I was curious as to where they went. A couple had some fairly useful information I couldn’t seem find by searching user names. I guess I need to refine my search more in depth.
 
I know there was a spat between Harold and Jon and Harold banned him and used what was called the nuclear option which either erased or renamed all of jon's posts. There are posts here with user name anonymous which may be jon and there are posts from anachronism which are still here and that was jon. it's just the posts from spaceships that I do not know for sure if they really still exist. Since the post count for spaceships is very low now they were somehow purged or that number would be higher.
 
I know there was a spat between Harold and Jon and Harold banned him and used what was called the nuclear option which either erased or renamed all of jon's posts. There are posts here with user name anonymous which may be jon and there are posts from anachronism which are still here and that was jon. it's just the posts from spaceships that I do not know for sure if they really still exist. Since the post count for spaceships is very low now they were somehow purged or that number would be higher.
You need to search for Anonymous, but not all are his.
There are others that received that attention from Harold.
 
I know there was a spat between Harold and Jon and Harold banned him and used what was called the nuclear option which either erased or renamed all of jon's posts. There are posts here with user name anonymous which may be jon and there are posts from anachronism which are still here and that was jon. it's just the posts from spaceships that I do not know for sure if they really still exist. Since the post count for spaceships is very low now they were somehow purged or that number would be higher.
I see now that that do not work.
 