- Joined
- May 31, 2016
- Messages
- 3,288
Time for a competition.
Rules: You get to ask your questions BEFORE you provide your answers. Once you put your answers in it's too late to ask again and you get one shot.
So now we have that out there here goes.
Here's a bag of 660 fuzzies.
Questions are as follows:
1. How long did it take (in hours) to get the gold into solution.
2. How many litres of solution did it take to get these into solution.
3. How much gold did I get?
4. How many litres of overall waste were generated? That includes solution, washing, everything.
I'd recommend asking a lot of questions BEFORE making your bids here guys. Let's have some fun.
For the record: A member already has all the answers and will not be guessing, that way it's all clear and transparent.
Rules: You get to ask your questions BEFORE you provide your answers. Once you put your answers in it's too late to ask again and you get one shot.
So now we have that out there here goes.
Here's a bag of 660 fuzzies.
Questions are as follows:
1. How long did it take (in hours) to get the gold into solution.
2. How many litres of solution did it take to get these into solution.
3. How much gold did I get?
4. How many litres of overall waste were generated? That includes solution, washing, everything.
I'd recommend asking a lot of questions BEFORE making your bids here guys. Let's have some fun.
For the record: A member already has all the answers and will not be guessing, that way it's all clear and transparent.