Hello everyone. I end up with a lot of low end scrap, and I am wondering if there is a cheap and simple way to recover non precious metals from the used HCL / AC / AR.
I do not have a chemistry background, and Google is not at all helpful in figuring things out.

A lot of the boards I get are low end - the copper and aluminum content is worth far more than the precious metals.
Metals I am interested in attempting to recover are metallic:
copper
aluminum
real tin
lead
nickle

Any help would be appreciated, thank you .
 
Crush those low end scrap and use gravitational method, such as shaking table will do.
 