S sayf Well-known member Joined Sep 1, 2020 Messages 139 Nov 14, 2022 #1 Hello guys, am working in a factory that recycle empty circuit boards, the output of this process is fiber copper and resin. Do you have any idea where or how to sell the fiber and resin product ? Thank you
Hello guys, am working in a factory that recycle empty circuit boards, the output of this process is fiber copper and resin. Do you have any idea where or how to sell the fiber and resin product ? Thank you
J Jado Well-known member Joined Nov 13, 2019 Messages 66 Nov 27, 2022 #2 Depends on the resin. Most resins are nearly impossible to remove, ecologically malignant, and a health hazard. True pyrolysis with hydrocarbon recapture would be the ideal solution, if the $$ isn’t an issue.
Depends on the resin. Most resins are nearly impossible to remove, ecologically malignant, and a health hazard. True pyrolysis with hydrocarbon recapture would be the ideal solution, if the $$ isn’t an issue.
Martijn Well-known member Joined Aug 3, 2014 Messages 2,591 Location Netherlands, Zeeland Nov 27, 2022 #3 https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6884634/It can be recycled for fiberglass fillers and more. Interesting article.
https://www.ncbi.nlm.nih.gov/pmc/articles/PMC6884634/It can be recycled for fiberglass fillers and more. Interesting article.