I want to recover gold with cyanide
From e waste please help me
Shahzad
Sent from my GT-I9060 using Tapatalk
From e waste please help me
Shahzad
Sent from my GT-I9060 using Tapatalk
I know cyanide is very dangerous. Thanks for advice. I will use Every precaution. If you have any processnickvc said:Welcome to the forum Muhammad.
One point to remember is that while cyanide is a useful tool in recovery it has its limitations such as only recovering visible gold and is also highly toxic.
Hi 4metals4metals said:Shahzad,
If you would like to be helped in your quest to refine gold from e-waste using cyanide it would be best if you told us something about your process and how you are currently processing your e-scrap. Do you have a system for collecting scrap components? Do you have any equipment to de-populate the boards and or granulate the boards? What is your final goal, gold and silver recovery or are you looking to recover copper as well?
Please describe what you have and how you plan to process this material. Why have you chosen cyanide as your best option? Cyanide is definitely an option, but not the only option.
When you get back with some details, you will get much more attention and help.
muhammad Shahzad said:Hi 4metals
First thing the cyanide is not my only choice. if any other chemical that is safe than cyenide most welcome but not aqua regia, acid proxide
And about the pcb de population i haven't need to de populate pcb i have telecom board that is gold plated. my purpose is to dissolve gold selectively with cyanide.
Now come to the gold recovery point
Please reply to me gold recovery process
Regards
Shahzad
Sent from my GT-I9060 using Tapatalk
4metals4metals said:Shahzad,
Are you looking to do this on a commercial scale or a hobby scale? The reason the answer is important is the approach you will need to take. Do you have any ability to measure concentrations of cyanide in solution?
Mr m.iftikharm.iftikhar447 said:Cyanide Process is Dangerous as you know and you have little bit knowledge about it. You should need more experience for that and this forum is best for new and professionals recyclers.
Have you tried burning process for telecom boards that is being used for commercial bases in region
Sent from my SM-J500H using Tapatalk
is really not appropriate. You are staring at a wonderful opportunity, but you have to play by our rules.If you describe cyanide gold recovery process it would be appropriate