When you comment a post, reply to it so we get the context right.sorry i needed to clarify that comment and i agree with you, ore that rich is ... well unheard of these days if ever
Hey guys. I recently bought some land in Cripple Creek Colorado and I think I may have a shit ton of calaverite. I'm waiting on my assay report. If it comes back positive. I'm going to need some help dealing with it in every aspect. I'm a complete green horn. And I would be genuinely and generously grateful. I'll check back in after Assay comes in.In all fairness - this may not be a scam - he posted -----
So he is not trying to sell out right - rather - he is interested in selling after having it analyzed
So he asked ----
And then he asked ----
So as I see it he is actually asking where to get an assay - & then asking where/how to sell - based on the assay
Hence my last question ---
If he has A LOT of it (as in tons of it) I would recommend Glencore or Mitsubishi
If he has a small amount (just a few specimens) it will be more difficult to put a deal together - but - we may then be able to teach him how to process it
Kurt
Welcome.Hey guys. I recently bought some land in Cripple Creek Colorado and I think I may have a shit ton of calaverite. I'm waiting on my assay report. If it comes back positive. I'm going to need some help dealing with it in every aspect. I'm a complete green horn. And I would be genuinely and generously grateful. I'll check back in after Assay comes in.
I absolutely would sell you some. I got lucky and found a hidden stash of it in an old Ore House. It was covered in rotting wood. I still have it all but haven't really been able to do much with it. I have had most of it at a Mill in Denver. Now I am seeing similar stuff on eBay which I think is mine. I find it and get ripped off. Sad. I still have a bunch though.Just curious how you got a couple tons. From the old open pit, or the new high grade to the North? I worked on the drill, when AK Drilling was in there doing reverse circulation for samples. Long before they started that pit. The average grade was 1 Troy per ton. I have heard there are pockets in it with almost pure Calaverite crystals. 1000's of Ozs. per ton. Not often, but spectacular when they occur. PM me if you are interested in selling a nice couple hundred dollar piece. I am in Colorado.
I am sorry about the no response. I haven't been in lately but I still have it. I've been putting it off forever while thieves have stole some and now I am seeing it on eBay.There is not a custom mill in the state. We have been trying to get the state to build a couple small mills throughout the state. These would facilitate cleaning up some older dumps, as well as help the small miner. No go, as of yet, but we are still trying.
No response from Dsrazstuntdriver, despite the offer to purchase a piece of the Cripple Creek ore with fluorite.
My stuff is from Cripple Creek. You said you was here last year. I didn't sell you a very rich piece did I? I miss that piece. It was the best one lol.Isn't this material located in the US, specifically Cripple Creek, CO? That area is known for tellurides and also hyperbolic estimates of grade, quantity, and moreover, ease of operating in the environment. I was just there last year.
Please contact me I would like to speak with you about your processI sell technology design especially for this. It's not cheap and i won't let you have it until payment is made. It uses nothing but household chemicals to remove the precious metals and is 100% environmentally friendly. I have people here who have tried it and are now millionaires.
With that much money on the line you can't afford not to buy my system. Win - Win!
Palladium has not been seen in over a year, and this post was an ironical reply to the OP.Please contact me I would like to speak with you about your process
ThanksPalladium has not been seen in over a year, and this post was an ironical reply to the OP.
Just curious how you got a couple tons. From the old open pit, or the new high grade to the North? I worked on the drill, when AK Drilling was in there doing reverse circulation for samples. Long before they started that pit. The average grade was 1 Troy per ton. I have heard there are pockets in it with almost pure Calaverite crystals. 1000's of Ozs. per ton. Not often, but spectacular when they occur. PM me if you are interested in selling a nice couple hundred dollar piece. I am in Colorado.
Sorry about that. I don't get on here as much as I should.There is not a custom mill in the state. We have been trying to get the state to build a couple small mills throughout the state. These would facilitate cleaning up some older dumps, as well as help the small miner. No go, as of yet, but we are still trying.
No response from Dsrazstuntdriver, despite the offer to purchase a piece of the Cripple Creek ore with fluorite.
If you are on Facebook, my name is Raymond Stacey FullerSorry about that. I don't get on here as much as I should.
AgreedHe eventually found his information, maybe.
Last time seen on the forum in December.
He is also from China, so buying the ore may be problematic.
We have developed a new method for telluride ores. I would be interested in checking your ore. We have an ICP-MS and deal with isotope stabilization.Hey guys. I recently bought some land in Cripple Creek Colorado and I think I may have a shit ton of calaverite. I'm waiting on my assay report. If it comes back positive. I'm going to need some help dealing with it in every aspect. I'm a complete green horn. And I would be genuinely and generously grateful. I'll check back in after Assay comes in.
He have not been on the forum since July last year.We have developed a new method for telluride ores. I would be interested in checking your ore. We have an ICP-MS and deal with isotope stabilization.
How can we obtain a sample?
Vesta Minerals Inc in Las Vegas, Nevada can assay the telluride ore by ICP-MS for precious metals and their isotopes of precious metals.I have some calaverite ore and I am finding who can extract the gold from this.
I am going to anaylsis specimen and then sell this ore.
Where can I anaylsis this specimen?
Where can I sell this calaverite?
If you are interesting, please contact me soon.
Thanks
If you hold the mouse cursor over the avatar of members it will show the last time they were logged in.Very Good
Vesta Minerals Inc in Las Vegas, Nevada can assay the telluride ore by ICP-MS for precious metals and their isotopes of precious metals.