diego Henrique vilela
Active member
Good morning to all friends. Does anyone have knowledge of palladium removal electrolysis cell? I have palladium-plated wires and I need to remove the palladium.
The base material Is cooper Bath Palladium plated.
I have 500 Kg this Is material , in anexed onde Photo.
The base material Is cooper Bath Palladium plated.
I have 500 Kg this Is material , in anexed onde Photo.