Ok I have my flame suit on already since this is probably a stupid question.
I have access to 90% platinum wire in bulk, It's coated but very thin coating, and sectioned in 4 inch pieces.
I know this stuff is a _______ to refine, so , I'm looking for ideas what to do with about 2 pounds of it. I can oxy/acetlyne melt it to ingots, but if there is something easier, I'm all ears. Maybe the O/A is the best route since it will burn off the shielding?
Open to whatever ideas.
I have access to 90% platinum wire in bulk, It's coated but very thin coating, and sectioned in 4 inch pieces.
I know this stuff is a _______ to refine, so , I'm looking for ideas what to do with about 2 pounds of it. I can oxy/acetlyne melt it to ingots, but if there is something easier, I'm all ears. Maybe the O/A is the best route since it will burn off the shielding?
Open to whatever ideas.