For those using SMB.

Instead of that smelly nasty horrible stuff, you might want to look into using Vitamin C instead. No odour, fast drops and less fumes from your waste. If you use Ferrous Sulphate for recovery drops and Vit C for refines you'll never need to use SMB ever again.

Vit C is Ascorbic acid. Available in large bags for a very similar price to SMB.
 