The answer is yes but I do not believe it's selective in which metal ions will precipitate, sulfur dioxide maybe used in the destruction of cyanide as will SMB added as a powder.

From 911 Metallurgist a list of other methods used to destroy cyanide.

I've decided to abandon activated carbon in favor of Electro-Oxidation onto steel wool as the latter serves two purposes.
 