Just wanted to say hi again and show off my progression of gold refining!
My latest nugget is my biggest yet at 26.19 grams, my target was 27 so I think I got pretty close! (Watch for scale) It took me a bit of collecting and gaining the courage to do such a big load of karat jewelry, about 55g of 10k, 12k, and 14k jewelry. I started off pretty rough by deciding to start with scrap electronics but I’m way more confident thanks to all of y’all!
I’m now totaling 46.88 grams of gold!!
I’m now doing both electronics and jewelry as they both are quite fun to me, it’s therapeutic to rip components of boards lol, maybe I’m weird!
I’ve also accumulated about a pound of silver as well, it still needs to go through another purification step though I think.
Hope you all enjoy!
My latest nugget is my biggest yet at 26.19 grams, my target was 27 so I think I got pretty close! (Watch for scale) It took me a bit of collecting and gaining the courage to do such a big load of karat jewelry, about 55g of 10k, 12k, and 14k jewelry. I started off pretty rough by deciding to start with scrap electronics but I’m way more confident thanks to all of y’all!
I’m now totaling 46.88 grams of gold!!
I’m now doing both electronics and jewelry as they both are quite fun to me, it’s therapeutic to rip components of boards lol, maybe I’m weird!
I’ve also accumulated about a pound of silver as well, it still needs to go through another purification step though I think.
Hope you all enjoy!