I don't know what is required in various countries to stamp bullion with a purity. I am sure it varies greatly.
 
Making bars is simple while coins are more work and investment and the point to remember is the buyers will not accept whatever you stamp on them as the truth, they will either test them and pay under spot or insist on refining them, so unless you have people who trust you to accept that stamp you are wasting effort and time.
As a way to keep your hard won rewards then make bars or shot.
 