Back yard Prospecting

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
After weeks soaking in Whink a lot of the gold started falling off the host rock. The gold particles weren't connected some fell off in chunks trying for a specimen. But we ended up with over 1- ounce so nice rock from a metal detector find.
 

Attachments

  • 20240204_085604.jpg
    20240204_085604.jpg
    544.8 KB · Views: 0
  • 8152DBFE-(1).jpg
    8152DBFE-(1).jpg
    419.9 KB · Views: 0
  • 20240501_121805.jpg
    20240501_121805.jpg
    1.6 MB · Views: 0
After weeks soaking in Whink a lot of the gold started falling off the host rock. The gold particles weren't connected some fell off in chunks trying for a specimen. But we ended up with over 1- ounce so nice rock from a metal detector find.
Are you crushing those? I bet you could get considerably more for it as a specimen, than crushing it just for the Au content.
 